护栏生锈先查焊点

来源:http://www.jnghbxg.com 日期:2026-11-06 发布人: 浏览次数:1次

铁艺护栏采购,别先挑花型。装上去头两年都好看,第三年焊口冒黄锈、竖杆根部脱皮,颜值救不了工艺。

When purchasing wrought iron guardrails, don't pick patterns first. It looks good in the first two years of installation, but in the third year, there is yellow rust on the welds and peeling at the base of the vertical pole, which cannot save the craftsmanship in terms of appearance.

17e655f9-9c9b-4822-8dfe-10c27fa22eb6

先卡基材和壁厚:

First, card the substrate and wall thickness:

立柱用Q235方管,壁厚≥1.8mm,受力处2.0mm以上;

The column is made of Q235 square tube, with a wall thickness of ≥ 1.8mm and a force bearing area of 2.0mm or more;

横杆≥1.2mm,竖杆≥0.8mm,薄壁空心管抗风抗撞都差;

Horizontal bars ≥ 1.2mm, vertical bars ≥ 0.8mm, and thin-walled hollow tubes have poor wind and impact resistance;

主受力件要材质证明,回收杂钢脆、易裂。

The main load-bearing components need material certification, and recycled miscellaneous steel is brittle and prone to cracking.

防锈顺序不能反:

The rust prevention sequence cannot be reversed:

只刷漆→2–3年锈点;冷镀锌→撑不过5年。正路是整体热浸锌(锌层≥65μm,户外按85μm)+环氧富锌底漆+静电喷塑,总干膜≥120μm。焊口、管口内壁必须补涂,只喷外面不补切口,内部先烂。

Paint only → 2-3 years rust spots; Cold galvanizing → can only last for 5 years. The main method is overall hot-dip galvanizing (zinc layer ≥ 65 μ m, outdoor according to 85 μ m)+epoxy zinc rich primer+electrostatic spraying, with a total dry film ≥ 120 μ m. The inner walls of welded joints and pipe openings must be repainted, only spraying the outside without repairing the incision, and the inside will rot first.

焊接是命门:

Welding is the gateway to life:

节点满焊,焊脚≥4mm,禁点焊虚焊。焊后清渣打磨,锌层破坏处补富锌漆。花件连接、竖杆根部、底口是重灾区。

Full welding of nodes, welding legs ≥ 4mm, no spot welding or virtual welding. Clean and polish the slag after welding, and apply rich zinc paint to the damaged zinc layer. Flower connections, vertical pole roots, and bottom openings are severely affected areas.

安装别省基础:

Install other provincial foundations:

优先混凝土预埋钢板,无预埋用M10以上化学锚栓,每柱≥4颗;

Priority should be given to embedding steel plates in concrete, and M10 or above chemical anchor bolts should be used without embedding. Each column should have at least 4 bolts;

立柱间距≤1.2m,垂直度≤3mm/m;

Column spacing ≤ 1.2m, verticality ≤ 3mm/m;

埋地基坑≥300mm,C25混凝土,底口留泄水孔不泡泥。

Buried foundation pit ≥ 300mm, made of C25 concrete, with drainage holes at the bottom without mud soaking.

安全尺寸卡强条:

Secure size card reinforcement strip:

临空<24m净高≥1.05m,≥24m按1.10m起;

When the clearance is less than 24m and the net height is greater than or equal to 1.05m, if it is greater than or equal to 24m, the minimum height shall be 1.10m;

竖杆净距≤110mm(托幼≤90mm),不设可踩踏水平横杆;

The clear distance between vertical poles is ≤ 110mm (kindergarten ≤ 90mm), and there is no horizontal horizontal bar that can be stepped on;

住宅水平荷载≥0.5kN/m,学校商业区1.0–1.5kN/m。

Residential horizontal load ≥ 0.5kN/m, school commercial area 1.0-1.5kN/m.

到货验收五摸:

Five touch inspection upon arrival:

卡尺量壁厚,不对样退;

Measure the wall thickness with a caliper and return the sample if it is not correct;

测厚仪抽锌层,切面不发黑;

The thickness gauge draws zinc layer, and the cut surface does not turn black;

划格法测附着力,不脱皮;

The grid method is used to measure adhesion without peeling;

摸焊口管口,无漏涂无毛刺;

Touch the welding port mouth, without any omissions or burrs;

摇顶部不晃、无异响。

Shake the top without shaking or abnormal noise.

合同写死:材质、壁厚、锌层μm、涂层工艺、锚固方式、质保年限。只报“XX元/米”的,辅料和补漆全在后头。

The contract specifies: material, wall thickness, zinc layer μ m, coating process, anchoring method, and warranty period. Only reporting "XX yuan/meter", all accessories and touch up paint are included at the back.

收口:护栏寿命=基材厚+锌层真+焊点补漆+基础锚死,四关过才叫能用十年。

Closing: The lifespan of the guardrail is equal to the thickness of the substrate, the zinc layer, the welding point repainting, and the foundation anchoring. It can only be used for ten years after passing four levels.